Using an innovative high-speed video setup, scientists in Germany were able to observe the screen-printing process used in solar cell metallization, on a time scale of less than 50 milliseconds. Insights into the paste’s behavior and the mechanisms at work during screen printing will improve the process and the formulation of the silver paste it relies on.

Solar cells use silver in the metallic ‘fingers’ screen printed onto their front sides, that transport charge generated in the silicon out into module and subsequently into the electricity system. Some experts predict that for solar to continue on its impressive growth trajectory, the industry will soon require most of the world’s silver production in order to keep making modules.

And while alternatives such as aluminum or copper are increasingly gaining ground, reducing the amount of silver consumed per cell offers a short-term solution. Hoping to achieve this by decreasing the width of the fingers and identifying alternative paste formulations that could achieve better conductivity with less silver, scientists at Germany’s Karlsruher Institute of Technology set out to gain a better understanding of how different paste compositions behave during the screen-printing process.

The group equipped an industrial screen printer (manufactured by Germany company ASYS) with a camera able to capture the process at 1,000 frames per second. The process was captured with two different paste compositions and various different process parameters, and the group went on to evaluate each one, looking at both the process video and the metallized cell itself. They presented their results in “Front side metallization of silicon solar cells – A high-speed video imaging analysis of the screen-printing process,” which was recently published in Solar Energy Materials and Solar Cells.

The study showed that in many cases, current commercial pastes rely on additives to achieve required morphology and printer compatibility. But these do not burn off completely, leaving behind residuals that can reduce paste conductivity. The group also observed multiple stages within the process, including paste spreading leading to (undesirable) increased line width.

KIT plans to continue this research with more paste compositions, and will particularly focus on varying wetting and flow properties in upcoming work. “This will enable the development of rational concepts stimulating further improvements of silver paste formulation for silicon solar cell front-side metallization,” the scientists said.

LEAVE A REPLY

Please enter your comment!
Please enter your name here

- Advertisment -

Most Popular

CLOU Electronics Sets New Safety Benchmark in Energy Storage with TS-800 Fire Test Certification

Energy storage has garnered unprecedented attention regarding its safety and reliability. On January 16, 2025, a fire broke out at the Moss Landing lithium...

E.ON cooperate with Superdielectrics to develop energy storage

E.ON is now working with a UK-based battery tech firm to advance more environmentally friendly energy storage for households. Energy utility giant E.ON has entered...

Trinasolar Unveils High-Power i-TOPCon Ultra Modules at Korea’s Green Energy Expo

Trinasolar, a global leader in smart PV and energy storage solutions, unveiled its revolutionary i‑TOPCon Ultra technology at Korea's Green Energy Expo in Daegu....

City of Fresno can’t stop adding solar and storage to city-owned sites

Today the City of Fresno Dept. of Public Utilities (DPU) in California conducted a “Flip the Switch” ceremony to celebrate the completion of solar...